COMMON PROBLEMS AND ANSWERS WHILE WHEELS USED IN THE PROCESS (1)
Source:
|
Author:hardware-66
|
Published time: 2018-01-24
|
2088 Views
|
Share:
QUESTION ONE: GLASS AFTER GRINDING BY THE DOUBLE EDGING MACHINE STILL HAVE COLLAPSE SIDE, OFF ANGLE, WHEEL PRINTING AND OTHER UNDESIRABLE PHENOMENA.
QUESTION ONE: GLASS AFTER GRINDING BY THE DOUBLE EDGING MACHINE STILL HAVE COLLAPSE SIDE, OFF ANGLE, WHEEL PRINTING AND OTHER UNDESIRABLE PHENOMENA.
ANSWER: THE CHOICE OF WHEEL GRIT IS NOT APPROPRIATE OR POOR PERFORMANCE, GRIT SHOULD BE ADAPTED TO THE PROCESSING OF GLASS THICKNESS AND PROCESSING SPEED REQUIREMENTS, SUCH AS 1, 2 GRINDING WHEELS ADOPT 80 MESH + 140 OR 180 MESH WHEN GRINDING 8MM-25MM GLASS IS GOOD, BUT GRINDING 5-6MM IT MAY COLLAPSE EDGE, THE GENERAL SHOULD CHOOSE 100 MESH +140 OR 180 MESH TO MEET THE REQUIREMENTS OF 4-19MM. ON THE OTHER HAND, IF THE GRINDING WHEEL NO. 1 ASSIGNED WITH A BIG AMOUNT OF GRINDING CAUSED A SMALL CHIPPING EDGE, ON THE 2ND, IT SHOULD BE ABLE TO SYNCHRONOUSLY CORRECT THE CHIPPED EDGE AND COMPLETELY COVER THE NO. 1 WEAR MARK. NO. 2 IS IGNORED FREQUENTLY AND THE PERFORMANCE OF THE SELECTION IS NOT GOOD. ALTHOUGH THE APPEARANCE IS NO. 1, REPLACE THE HIGH-PERFORMANCE NO. 2 WHEEL AND RE-COMMISSION REASONABLE OF THE GRINDING AMOUNT IS NECESSARY.